Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Dyneon™ PFA 6502TA Perfluoroalkoxy Fluorothermoplastic  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PFA
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ PFA 6502TA Perfluoroalkoxy Fluorothermoplastic  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dyneon PFA 6502TA is a fluorothermoplastic resin developed for compression molding applications. PFA 6502TA has a wide processing window with excellent color stability when longer residence times or higher temperatures are required.Information provided by Dyneon, A 3M Company
Physical Properties Metric English Comments
Specific Gravity 2.15 g/cc
2.15 g/cc
ASTM D792
Bulk Density 0.850 g/cc
0.0307 lb/in³
DIN 53466
Melt Index of Compound 2.0 g/10 min

@Load 5.00 kg,
Temperature 372 °C
2.0 g/10 min

@Load 11.0 lb,
Temperature 702 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength at Break 30.0 MPa
4350 psi
ASTM D638
Elongation at Break 380 %
380 %
ASTM D638
Flexural Modulus 0.550 GPa
79.8 ksi
ASTM D790
Thermal Properties Metric English Comments
Melting Point 308 °C
586 °F
ASTM D4591
Oxygen Index >= 95 %
>= 95 %
ASTM D2863
Descriptive Properties Value Comments
Form Agglomerate
Users viewing this material also viewed the following: