Material Notes:
Used for impregnation.Dyneon PTFE dispersions are aqueous dispersions developed for use in metal coating formulations and for application of impregnation and fabric coating applications. A range of products are offered to meet the variety of requirements for particle size, emulsifier type and content, and solids level.Data provided by Dyneon.
Physical Properties Metric English Comments
Density 1.50 g/cc
0.0542 lb/in³
hydrometer
Solids Content 60 %
60 %
ASTM D4441
Particle Size 160 µm
160 µm
ISO 13321
pH 8.5
8.5
ASTM D4441
Viscosity 22 cP
22 cP
D=30/s; DIN 54 453
Descriptive Properties Value Comments
Emulsifier Content 5%
ASTM D4441
Emulsifier Type non-ionic