3M Dyneon™ TF 5041 PTFE Dispersion  (discontinued **)

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Dyneon™ TF 5041 PTFE Dispersion  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PTFE dispersion with micro glass spheres for membrane structures.Information provided by the Dyneon division of 3M.
Physical Properties Metric English Comments
Specific Gravity 1.40 g/cc
1.40 g/cc
hydrometer
Solids Content 60 %
60 %
ASTM D4441
Particle Size 225 µm
225 µm
ISO 13321
pH 9.0
9.0
ASTM D4441
Viscosity 47 cP
47 cP
D=30/s; DIN 54 453
Descriptive Properties Value Comments
Emulsifier Content (%) 8
ASTM D4441
Emulsifier Type non-ionic