3M FP017102 White Polyester Label Products

Category Polymer , Adhesive
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M FP017102 White Polyester Label Products.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ White Polypropylene Label Products FP017102 and FP026508 offer excellent durability and moisture resistance. These label products utilize 3M™ Adhesive P1110, which is a general purpose permanent rubber-based adhesive that exhibits quick tack and high ultimate adhesion to a wide variety of surfaces, including polyolefins.Information provided by 3M
Physical Properties Metric English Comments
Thickness 66.0 microns
2.60 mil
Facestock
78.7 microns
3.10 mil
Liner
Mechanical Properties Metric English Comments
Peel Strength 0.701 kN/m
4.00 pli
180° Peel, 12"/min., 1" wide sample; TLMI Method
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 43.0 °C
109 °F
Application
60.0 °C
140 °F
Service
Minimum Service Temperature, Air 5.00 °C
41.0 °F
Service
13.0 °C
55.4 °F
Application
Processing Properties Metric English Comments
Shelf Life 24.0 Month
24.0 Month
Descriptive Properties Value Comments
Adhesive Type P1110 Perm 23
Appearance 50# SC