3M Novec™ 72DA Engineered Fluid

Category Fluid
Manufacturer 3M
Trade Name Novec™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Novec™ 72DA Engineered Fluid.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Novec™ 72DA is ideal for flux removal and vapor degreasing operations. It is non-flammable and low in toxicity which makes it an ideal replacement for chlorinated solvents such as Trichloroethylene (TCE) and for n-propyl bromide (nPB).Feature and Benefits:Non-flammable Non-conductive Low toxicity Low Global Warming Potential (GWP) Zero ozone depletion potential Low surface tension penetrates tight spaces for improved cleaning Excellent for removal of ionic contaminationInformation provided by 3M
Physical Properties Metric English Comments
Density 1.27 g/cc
0.0459 lb/in³
Liquid
Viscosity 0.40 cP
0.40 cP
Vapor Pressure 0.480 bar
360 torr
Surface Tension 18 dynes/cm
18 dynes/cm
Thermal Properties Metric English Comments
Heat of Vaporization 251.2 J/g
108.1 BTU/lb
Boiling Point 44.0 °C
111 °F