Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M RPF-CWR (0.417 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane Foam, Unreinforced
Manufacturer 3M
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M RPF-CWR (0.417 g/cc) (Reinforced Polyurethane Foam) Continuous Strand Fiberglass with Woven Roving.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ RPF-C (Reinforced Polyurethane Foam) is a polyurethane foam with layers of continuous strand fiberglass and woven roving throughout the polyurethane. The composites are 30% to 45% lighter than plywood, have a high strength-to-weight ratio, very low water absorption (1.0% or less) and will not have any water rot or insect infestation.Information provided by 3M
Physical Properties Metric English Comments
Water Absorption 1.1 %
1.1 %
ASTM C272
Mechanical Properties Metric English Comments
Tensile Strength at Break 1900 MPa
276000 psi
ASTM C297
Flexural Strength 29.84 MPa
4328 psi
ASTM D790
Flexural Modulus 1.93 GPa
280 ksi
ASTM D790
Compressive Strength 0.641 MPa
93.0 psi
Core; ASTM C365
Compressive Modulus 0.13734 GPa
19.919 ksi
Core; ASTM C365
Shear Modulus 0.03265 GPa
4.735 ksi
Core; ASTM C273
Shear Strength 4.01 MPa
582 psi
Core; ASTM C273
Users viewing this material also viewed the following: