3M Scotch® 202 Paper Masking Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 202 Paper Masking Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Paper Masking Tape 202 is a high performance, excellent paint masking tape for holding, protecting and bundling where a pressure sensitive tape is needed.Information provided by 3M
Physical Properties Metric English Comments
Thickness 160 microns
6.30 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 29.5 MPa
4280 psi
ASTM D3756
Elongation at Break 8.0 %
8.0 %
ASTM D3756
Processing Properties Metric English Comments
Shelf Life 12.0 Month
12.0 Month
Descriptive Properties Value Comments
Adhesive Type Rubber
Appearance Tan