Material Notes:
Scotch® High Performance Masking Tape 2693 is a smooth, heavy duty, mini-crepe paper masking tape suitable for most paint masking applications. Designed for automotive, truck and bus applications where very aggressive room temperature and high temperature holding is require.Information provided by 3M
Physical Properties Metric English Comments
Thickness 5.08 microns
0.200 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 25.75 MPa
3735 psi
ASTM D3759
Elongation at Break 10 %
10 %
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
to Steel; ASTM D3330
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 163 °C
325 °F
for 30 mins
Descriptive Properties Value Comments
Adhesive Type Synthetic rubber
Appearance Tan