3M Scotch® 600 Transparent Film Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 600 Transparent Film Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Tape 600 is a transparent film tape that is excellent for various packaging applications. It has a pressure sensitive acrylic adhesive system which is long aging and highly transparent, so it has stain and sunlight resistance which makes it an excellent choice for use on fabrics. Recommended for gift-wrapping, combining, attaching, light duty carton sealing and miscellaneous store use.Information provided by 3M
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Backing; ASTM D3652
58.4 microns
2.30 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Elongation at Break 45 %
45 %
ASTM D3759
Peel Strength 0.438 kN/m
2.50 pli
Adhesion to Steel; ASTM D3330
Film Tensile Strength at Break, MD 8.45 MPa
1230 psi
ASTM D3759
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive acrylic
Appearance Transparent