3M Scotch® 690 Colored Film Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 690 Colored Film Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Tape 690 is a colored film tape featuring a durable, moisture- and chemical- resistant 3M™ Paklon™ film backing with a rubber resin adhesive. This decorative film is excellent for various packaging, color-coding, bag sealing, combining, and attaching applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 38.1 microns
1.50 mil
Backing; ASTM D3652
58.4 microns
2.30 mil
Total; ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.6 MPa
1530 psi
Longitudinal; ASTM D3759
Elongation at Break 45 %
45 %
ASTM D3759
Peel Strength 0.3287 kN/m
1.875 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive rubber resin
Appearance Black, blue, green, red, white and yellow