3M Scotch® 880MSR Filament Tape

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotch®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotch® 880MSR Filament Tape.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotch® Filament Tape 880MSR is a high performance transparent filament tape reinforced along its length with continuous polyester-yarn filaments, which gives the tape a very high tensile strength. The clear polyester backing provides excellent abrasion, moisture and scuff resistance. The adhesive is a modified synthetic rubber resin adhesive specifically formulated to provide very good oily metal adhesion performance. The adhesive also provides a balanced performance having high adhesion and long term holding power for a variety of metal working applications.Information provided by 3M
Physical Properties Metric English Comments
Thickness 196 microns
7.70 mil
ASTM D3652
Mechanical Properties Metric English Comments
Tensile Strength at Break 23.6 MPa
3430 psi
ASTM D3759
Elongation at Break 19 %
19 %
ASTM D3759
Peel Strength 1.0408 kN/m
5.9375 pli
Adhesion to Steel; ASTM D3330
Descriptive Properties Value Comments
Adhesive Type Pressure sensitive modified synthetic rubber resin
Appearance Clear