Material Notes:
3M™ Scotch-Weld™ Neoprene High Performance Contact Adhesive can be used to bond most rubber, cloth, metal, wood, foamed glass, paper honeycomb, decorative plastic laminates and many other substrates.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 17 - 19 %
17 - 19 %
Brookfield Viscosity 35 - 65 cP
35 - 65 cP
RVF #1 sp @ 20 rpm @ 80°F
Mechanical Properties Metric English Comments
Shear Strength 1.09 MPa

@Temperature 107 °C,
Time 1.81e+6 sec
158 psi

@Temperature 225 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
1.37 MPa

@Temperature 82.0 °C,
Time 1.81e+6 sec
199 psi

@Temperature 180 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
3.12 MPa

@Temperature 75.0 °C,
Time 1.21e+6 sec
452 psi

@Temperature 167 °F,
Time 336 hour
Overlap, 1/8" Birch/Birch
3.70 MPa

@Temperature 75.0 °C,
Time 1.81e+6 sec
536 psi

@Temperature 167 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
6.65 MPa

@Temperature -34.0 °C,
Time 1.81e+6 sec
964 psi

@Temperature -29.2 °F,
Time 504 hour
Overlap, 1/8" Birch/Birch
Peel Strength 2.10 kN/m

@Temperature 82.0 °C,
Time 1.81e+6 sec
12.0 pli

@Temperature 180 °F,
Time 504 hour
180°, Canvas/Steel
2.28 kN/m

@Temperature -34.0 °C,
Time 1.81e+6 sec
13.0 pli

@Temperature -29.2 °F,
Time 504 hour
180°, Canvas/Steel
2.80 kN/m

@Temperature 24.0 °C,
Time 86400 sec
16.0 pli

@Temperature 75.2 °F,
Time 24.0 hour
180°, Canvas/Steel
3.24 kN/m

@Temperature 66.0 °C,
Time 1.81e+6 sec
18.5 pli

@Temperature 151 °F,
Time 504 hour
180°, Canvas/Steel
4.03 kN/m

@Temperature 24.0 °C,
Time 1.81e+6 sec
23.0 pli

@Temperature 75.2 °F,
Time 504 hour
180°, Canvas/Steel
4.21 kN/m

@Temperature 24.0 °C,
Time 1.21e+6 sec
24.0 pli

@Temperature 75.2 °F,
Time 336 hour
180°, Canvas/Steel
4.56 kN/m

@Temperature 24.0 °C,
Time 605000 sec
26.0 pli

@Temperature 75.2 °F,
Time 168 hour
180°, Canvas/Steel
5.43 kN/m

@Temperature 24.0 °C,
Time 259000 sec
31.0 pli

@Temperature 75.2 °F,
Time 72.0 hour
180°, Canvas/Steel
7.36 kN/m

@Temperature 24.0 °C,
Time 432000 sec
42.0 pli

@Temperature 75.2 °F,
Time 120 hour
180°, Canvas/Steel
Thermal Properties Metric English Comments
Flash Point -26.0 °C
-14.8 °F
TCC
Descriptive Properties Value Comments
Appearance Gray/Green
Base Polychloroprene