Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

3M Scotchcast™ 5400 Electrical Powder Resin

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer 3M
Trade Name Scotchcast™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchcast™ 5400 Electrical Powder Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M Scotchcast Electrical Resin 5400 has been specially developed for continuous coating process. It is well suited for applications where flexibility and resistance to cracking due to heat shock or impact are required. Scotchcast 5400 is manufactured by a fusion blend process which insures that each individual particle of powder contains all the components necessary to effect a complete cure and attain the stated performance characteristics.Information provided by 3M
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
cured; ASTM D794
Thermal Properties Metric English Comments
Thermal Conductivity 0.270 W/m-K
1.87 BTU-in/hr-ft²-°F
Electrical Properties Metric English Comments
Dielectric Constant 3.8

@Frequency 100 Hz,
Temperature 25.0 °C
3.8

@Frequency 100 Hz,
Temperature 77.0 °F
4.5

@Frequency 100 Hz,
Temperature 150 °C
4.5

@Frequency 100 Hz,
Temperature 302 °F
Dissipation Factor 0.50

@Frequency 100 Hz,
Temperature 25.0 °C
0.50

@Frequency 100 Hz,
Temperature 77.0 °F
0.50

@Frequency 100 Hz,
Temperature 150 °C
0.50

@Frequency 100 Hz,
Temperature 302 °F
after 18 hours
Processing Properties Metric English Comments
Dry Time 0.333 hour
0.333 hour
50% RH
Gel Time 0.250 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 204 °C
0.250 - Error in fixSigDigits: @digits must be between 1 and 12. @digits is: 15 min

@Temperature 399 °F
Descriptive Properties Value Comments
Appearance Yellow/Tan