3M Scotchgard™ 1002MS Multi-Layer Protective Films

Category Polymer , Adhesive
Manufacturer 3M
Trade Name Scotchgard™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchgard™ 1002MS Multi-Layer Protective Films.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
3M™ Scotchgard™ Multi-Layer Protective Films 1002MS is optically transparent, pressure-sensitive polyester film tapes designed to protect surface from intentional and unintentional damage caused by scratching, etching, abrasion and graffiti. A damaged film layer can be quickly and easily removed, exposing a fresh protective sheet.Information provided by 3M
Physical Properties Metric English Comments
Thickness 246 microns
9.70 mil
ASTM D3652
Mechanical Properties Metric English Comments
Peel Strength 0.307 kN/m
1.75 pli
Base Layer Adhesion to Polycarbonate; ASTM D3330
0.31773 kN/m
1.8125 pli
Base Layer Adhesion to Glass; ASTM D3330
Optical Properties Metric English Comments
Haze 2.0 %
2.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003
Descriptive Properties Value Comments
Adhesive Type Acrylic
Clarity 0.97
ASTM D1003