3M Scotchgard™ Resilient Floor Protector

Category Polymer
Manufacturer 3M
Trade Name Scotchgard™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchgard™ Resilient Floor Protector.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchgard Resilient Floor Protector is a high performance protective floor coating for vinyl tile and vinyl sheet flooring that utilizes multiple polymer technologies to produce a hard surface that is resistant to scratches, stains, and scuff marks.Information provided by 3M
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
Solids Content 22 %
22 %
Volatile Organic Compounds (VOC) Content <= 1.0 g/l
<= 1.0 g/l
pH 7.4 - 8.4
7.4 - 8.4
Viscosity <= 8.0 cP
<= 8.0 cP
Thermal Properties Metric English Comments
Boiling Point >= 35.0 °C
>= 95.0 °F
Descriptive Properties Value Comments
Appearance White Liquid