3M Scotchkote™ 60EG 533 Urethane Elastomer

Category Polymer , Thermoset , Polyurethane, TS , Thermoset Polyurethane, Elastomer, Unreinforced
Manufacturer 3M
Trade Name Scotchkote™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF 3M Scotchkote™ 60EG 533 Urethane Elastomer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Scotchkote Urethane Elastomer 60EG 533 has been specifically developed as an elastomeric repair system with a high degree of flexibility for rebuilding and resurfacing rubber components.Product Features:Physical properties similar to factory produced rubbersDeigned for application by trowel or spatula at thicknesses up to 6 mmGood cold vulcanizing capabilitiesSuitable for use to repair conveyor belts, rollers, gaskets, hoses, etc.Information provided by 3M
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Volatile Organic Compounds (VOC) Content 0.00 g/l
0.00 g/l
Thickness 6100 microns
240 mil
Mechanical Properties Metric English Comments
Hardness, Shore A 60
60
Tensile Strength at Break 6.89 MPa
999 psi
Elongation at Break 800 %
800 %
Electrical Properties Metric English Comments
Dielectric Strength 16.0 kV/mm
406 kV/in
Processing Properties Metric English Comments
Cure Time 180 min
3.00 hour
Initial Set
960 min
16.0 hour
Machining Time
4320 min
72.0 hour
Full Mechanical
Descriptive Properties Value Comments
Appearance Black