Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Impact Modified; Molded/Extruded
Manufacturer A. Schulman, Inc.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF A. Schulman PP 3052X-01 Polypropylene Impact Resistant Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
DescriptionPolypropylene PP 3052X-01 is an extra high flow impact resistant copolymer with relatively high stiffness. Information provided by A. Schulman.
Physical Properties Metric English Comments
Specific Gravity 0.900 g/cc
0.900 g/cc
ASTM D792
Melt Flow 30 - 35 g/10 min

@Load 2.16 kg,
Temperature 230 °C
30 - 35 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 27.6 MPa
4000 psi
2 in/min; ASTM D638
Flexural Modulus 1.24 GPa
180 ksi
ASTM D790
Izod Impact, Notched 0.747 J/cm
1.40 ft-lb/in
ASTM D256
Gardner Impact 2.26 J

@Temperature -28.9 °C
1.67 ft-lb

@Temperature -20.0 °F
ASTM D5420
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 106 °C
223 °F
ASTM D648