Material Notes:
Part of the Amber Chemical Group. Data provided by manufacturer.
Physical Properties Metric English Comments
Density 0.104 g/cc
0.00376 lb/in³
ASTM D1056
Mechanical Properties Metric English Comments
Tensile Strength, Yield 0.0827 MPa
12.0 psi
ASTM D412
Elongation at Break 100 %
100 %
ASTM D412
Compression Set 0.00 %
0.00 %
at 50%, 22 hrs @ 70°C; ASTM D1056
0.00 %

@Temperature 100 °C
0.00 %

@Temperature 212 °F
at 50%, 22 hrs; ASTM D1056
Thermal Properties Metric English Comments
Flammability Test <= 25
<= 25
ASTM E162/D 3675
Smoke Density 1.5 min
1.5 min
<20; ASTM E662
4.0 min
4.0 min
<50; ASTM E662
Descriptive Properties Value Comments
Durability 0% Height Loss
Jounce & Squirm (1,000,000 cycles)
IFD, lbs 35
ASTM S3574 B1 @ 1" thick
Noise Reduction-Coefficient 0.65
ASTM C423-90a
Thermal Resistance, ft2-h/BTU 2.7
ASTM C518
Toxic Gas Emission Pass
Bombardier SMP 800C
Vertical Flammability Pass
FAR25.83(a)(1)(i) 12sec
Pass
FAR25.83(a)(1)(i) 60sec
Users viewing this material also viewed the following: