Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® AEN 6000-1 Nylon 6 Engineered Resin

Category Polymer , Thermoplastic , Nylon , Nylon 6
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® AEN
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® AEN 6000-1 Nylon 6 Engineered Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Specific Gravity 1.14 g/cc
1.14 g/cc
ASTM D792
Linear Mold Shrinkage 0.012 cm/cm
0.012 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 81.4 MPa
11800 psi
ASTM D638
Flexural Modulus 2.74 GPa
398 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 182 °C
360 °F
ASTM D648
Users viewing this material also viewed the following: