Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® AEPC 5000-3 Engineered Polycarbonate Resin

Category Polymer , Thermoplastic , Polycarbonate (PC)
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® AEPC
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® AEPC 5000-3 Engineered Polycarbonate Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Melt flow index may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.20 g/cc
1.20 g/cc
ASTM D792
Linear Mold Shrinkage 0.0050 - 0.0070 cm/cm
0.0050 - 0.0070 in/in
ASTM D955
Melt Flow 15 g/10 min

@Load 2.16 kg,
Temperature 230 °C
15 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength 60.7 MPa
8800 psi
ASTM D638
Flexural Modulus 2.41 GPa
350 ksi
ASTM D790
Izod Impact, Notched 8.01 J/cm
15.0 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 129 °C
265 °F
ASTM D648