Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound

Category Polymer , Thermoplastic , Elastomer, TPE , Thermoplastic Elastomer, Melt-Processible Rubber
Manufacturer Aaron Industries Corporation
Trade Name AAROPRENE® ATPR
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aaron Industries AAROPRENE® ATPR 1000 60A Elastomeric Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AAROPRENE® ATPR 1000 Series Elastomeric CompoundDurometer values may be specified. Color may be specified.
Physical Properties Metric English Comments
Specific Gravity 1.00 - 1.10 g/cc
1.00 - 1.10 g/cc
ASTM D792
Melt Flow 80 g/10 min

@Load 2.16 kg,
Temperature 190 °C
80 g/10 min

@Load 4.76 lb,
Temperature 374 °F
"E"; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 57 - 63
57 - 63
ASTM D2240
Tensile Strength 6.07 MPa
880 psi
ASTM D412
Elongation at Break 625 %
625 %
ASTM D412
Tensile Modulus 0.00207 GPa
0.300 ksi
ASTM D412
Tear Strength 31.6 kN/m
180 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 355
355
H-18; ASTM D1044
Users viewing this material also viewed the following: