Material Notes:
5% filled gray colored casting and adhesive resin; solventless. 2/1 ratio.Information provided by Abatron.
Physical Properties Metric English Comments
Filler Content 5 %
5 %
Mechanical Properties Metric English Comments
Hardness, Shore D 80
80
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 50.0 °C
122 °F
Processing Properties Metric English Comments
Pot Life >= 60 min
>= 60 min
Descriptive Properties Value Comments
Color Gray
Viscosity Low