Material Notes:
2-part solvent-free dielectric epoxy casting compound.Processing: 100/13.2 ratio (pbw); Gel time, 100 g (3.5 oz.): 49 minutes; cures in 16 hours at 25°C (77°F); postcure: 2 hours at 100°C (212°F).Applications: solventless casting, adhesive, and coating.
Physical Properties Metric English Comments
Water Absorption 0.21 %
0.21 %
in 24 hours.
Viscosity Measurement 400
400
Mechanical Properties Metric English Comments
Hardness, Shore D 87
87
Tensile Strength, Ultimate 73.77 MPa
10700 psi
Elongation at Break 5.9 %
5.9 %
Flexural Strength 134.45 MPa
19500 psi
Izod Impact, Notched 0.262 J/cm
0.491 ft-lb/in
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 77.0 °C
171 °F
Deflection temperature; load unknown.
Electrical Properties Metric English Comments
Electrical Resistivity 7.00e+10 ohm-cm

@Temperature 93.3 °C
7.00e+10 ohm-cm

@Temperature 200 °F
3.00e+13 ohm-cm

@Temperature 65.6 °C
3.00e+13 ohm-cm

@Temperature 150 °F
8.00e+13 ohm-cm

@Temperature 25.0 °C
8.00e+13 ohm-cm

@Temperature 77.0 °F
Dielectric Constant 4.0

@Frequency 1e+6 Hz
4.0

@Frequency 1e+6 Hz
Dissipation Factor 0.020

@Frequency 1e+6 Hz
0.020

@Frequency 1e+6 Hz
Processing Properties Metric English Comments
Processing Temperature 25.0 °C
77.0 °F
Curing time: 16 hours; Postcure: 2 hours/100°C (212°F)