Abatron AboSeal 8104-14 Polysulfide, Thixotropic Sealant and Caulk

Category Polymer , Adhesive , Thermoset
Manufacturer Abatron
Trade Name AboSeal
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron AboSeal 8104-14 Polysulfide, Thixotropic Sealant and Caulk.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
AboSeal 8104-14 is a 2-part, 100% solids, thixotropic polysulfide. It only comes in black. It is great for expansion joints on floors and decks with heavy traffic. It is a structural, heavy-duty standard for architectural, industrial, and marine applications. It has the highest combination of toughness, elongation, and tensile strength.
Physical Properties Metric English Comments
Solids Content 100 %
100 %
Mechanical Properties Metric English Comments
Hardness, Shore A 61
61
Tensile Strength at Break 3.48 MPa
505 psi
Elongation at Break 620 %
620 %
Descriptive Properties Value Comments
Color Black
Parts by Weight (pbw) 10
Part B
100
Part A