Material Notes:
BestBond® is a versatile adhesive designed for both interior and exterior wood projects. BestBond® is water-resistant, easy to clean up, non-toxic, and flexible. Primary suggested uses include furniture assembly and repair, cabinetry, stairs and floors, window/door frames and seals, woodcraft, and toys. It is also used to bond any dry, porous materials such as paper, fabric, leather, carpets, and all wood materials. It can be applied by brushing, pouring or spraying. BestBond® is a translucent liquid, which hardens clear and bubble-free. BestBond® is tack-free in twenty minutes, allowing ample time for adjustments in position of parts or even their complete re-assembly.
Physical Properties Metric English Comments
Specific Gravity 1.06 g/cc
1.06 g/cc
Volatile Organic Compounds (VOC) Content 335.5 g/l
335.5 g/l
Viscosity 100 - 400 cP
100 - 400 cP
Mechanical Properties Metric English Comments
Tensile Strength at Break 40.7 MPa
5900 psi
Elongation at Break 190 %
190 %
Tensile Modulus 0.0296 GPa
4.30 ksi
at yield point
Adhesive Bond Strength 8.89 MPa
1290 psi
Descriptive Properties Value Comments
Green Strength (min) 60
Hardness, pencil 2H
Tack-free Time (min) 20
Users viewing this material also viewed the following: