Abatron Water Epoxy Floor Coating System

Category Polymer , Adhesive , Thermoset , Epoxy , Epoxy Adhesive
Manufacturer Abatron
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Abatron Water Epoxy Floor Coating System.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
The Water Epoxy Floor Coating System combines beauty, durability, slip resistance, ease of application, and water resistance. Its other features and benefits include low odor on installation, easy maintenance, and unlimited standard and custom color options. The high gloss system is ideal for hospitals, playrooms, utility rooms, basements, and high-traffic walking surfaces. It is recommended for indoor use. The system includes a colored base coat, vinyl color chips, and an acrylic topcoat.
Physical Properties Metric English Comments
Volatile Organic Compounds (VOC) Content 257.6 g/l
257.6 g/l
EPA method #24
Mechanical Properties Metric English Comments
Adhesive Bond Strength 2.05 MPa
298 psi
ASTM-D4541
Coefficient of Friction 1.3
1.3
Slip resistance; ASTM-D1894
Thermal Properties Metric English Comments
Flash Point 100 °C
212 °F
ASTM-D3278
Descriptive Properties Value Comments
Abrasive Resistance (g) 0.101
ASTM-D4060; CS 17/Load 1000/Cycles 1000
Hardening Time (min) 120