Material Notes:
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0010 cm/cm
0.0010 in/in
MD; ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 109
109
ASTM D785
Tensile Strength at Break 170.0 MPa
24650 psi
ASTM D638
Tensile Strength, Yield 170.0 MPa
24650 psi
ASTM D638
Elongation at Break 7.0 %
7.0 %
ASTM D638
Elongation at Yield 5.0 %
5.0 %
ASTM D638
Tensile Modulus 4.599 GPa
667.1 ksi
ASTM D638
Flexural Strength 263.0 MPa
38140 psi
ASTM D790
Flexural Modulus 11.298 GPa
1638.7 ksi
ASTM D790
Izod Impact, Notched 1.76 J/cm
3.30 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 200 °C
392 °F