Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Aclo Accutech Polypropylene Homopolymer HP0334M20CL Mica Reinforced Coupled

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 20% Mica Filler
Manufacturer Aclo Compounders
Trade Name Accutech
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aclo Accutech Polypropylene Homopolymer HP0334M20CL Mica Reinforced Coupled.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Physical Properties Metric English Comments
Density 1.03 g/cc
0.0372 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0090 cm/cm
0.0090 in/in
MD; ASTM D955
Melt Flow 3.0 g/10 min
3.0 g/10 min
ASTM D1238
Ash 20 %
20 %
ASTM D2584
Mechanical Properties Metric English Comments
Hardness, Rockwell R 65
65
ASTM D785
Tensile Strength at Break 26.0 MPa
3770 psi
ASTM D638
Tensile Strength, Yield 35.0 MPa
5080 psi
ASTM D638
Elongation at Break 17 %
17 %
ASTM D638
Elongation at Yield 6.0 %
6.0 %
ASTM D638
Tensile Modulus 2.299 GPa
333.5 ksi
ASTM D638
Flexural Strength 43.0 MPa
6240 psi
ASTM D790
Flexural Modulus 2.299 GPa
333.5 ksi
ASTM D790
Izod Impact, Notched 0.587 J/cm
1.10 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 113 °C
235 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 65.0 °C
149 °F