Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Addcomp ADD-VANCE® AS 838 Anti-static masterbatch, PP based

Category Other Engineering Material , Additive/Filler for Polymer , Polymer , Thermoplastic , Polypropylene (PP)
Manufacturer Addcomp
Trade Name ADD-VANCE®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Addcomp ADD-VANCE® AS 838 Anti-static masterbatch, PP based.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fields of application: Highly loaded anti-static masterbatch for polypropylene.Examples: Thermoformed and injection molded PP products such as margarine containers and other packaging products. Other applications are films, sheets, tapes, yarns, fibers and household products.Mode of action and advantages: ADD-VANCE AS 838 contains an effective, fast migrating anti-static additive.Advantages: Immediate anti-static protection after production of the PP article; Safe to use as a result of the food contact approved anti-static formulation; Excellent de-moulding properties for injection molded products; Good cost economy; Non-sticking pellets, dust free dosing; and Safe and easy handling.Regulations: ADD-VANCE AS 838 is very suitable for food packaging products as the active ingredients are in compliance with current food contact regulations.Information provided by ADDCOMP
Processing Properties Metric English Comments
Processing Temperature <= 280 °C
<= 536 °F
Descriptive Properties Value Comments
Appearance White/off-white granules
Dosing Level 0.008
Users viewing this material also viewed the following: