Material Notes:
Initiator for the (co)polymerization of styrene, acrylonitrile, vinylchloride, vinylidenechloride, acrylates and methacrylates. Trigonox A-W70 may also be used as an initiator for the room temperature cure of promoted unsaturated polyester and vinylester resins, and elevated cure of non-promoted resins.Chemical Description: tert-Butyl hydroperoxide, 70% solution in waterCAS Number: 75-91-2Acronym: TBHP; Tx A-W70Information provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
One Hour Half Life Temperature 185 °C
365 °F
Storage Temperature 0.000 - 40.0 °C
32.0 - 104 °F