Akzo Nobel Trigonox® T-50D-pd Peroxide Cure Agent

Category Other Engineering Material , Catalyst/Initiator , Polymer
Manufacturer Akzo Nobel
Trade Name Trigonox®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Akzo Nobel Trigonox® T-50D-pd Peroxide Cure Agent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Trigonox T-50D-pd is a monofunctional peroxide which is used for the crosslinking of polyolefins as well as natural rubber and synthetic rubbers. Chemical Description: tert-Butyl cumyl peroxide, powder, 50% with inert fillersCAS Number: 3457-61-2Acronym: TBCP; Tx TInformation provided by Akzo Nobel Polymer Chemicals.
Physical Properties Metric English Comments
One Hour Half Life Temperature 146 °C
295 °F
Storage Temperature <= 40.0 °C
<= 104 °F