AlphaGary Megolon™ HF 8037 DD Low Smoke Halogen Free

Category Polymer , Thermoplastic
Manufacturer AlphaGary
Trade Name Megolon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Megolon™ HF 8037 DD Low Smoke Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
MEGOLON™ HF 8037 DD is a low die drool, flame retarded, zero halogen jacketing compound
Mechanical Properties Metric English Comments
Tensile Strength 11.7 MPa
1700 psi
Elongation at Break 300 %
300 %
ASTM D412
Thermal Properties Metric English Comments
Oxygen Index 40 %
40 %