Material Notes:
Highly fire retardant compound for use in demanding fire tests and constructions. Application examples include Data Cables, Optical Cables.
Mechanical Properties Metric English Comments
Tensile Strength 12.0 MPa
1740 psi
Elongation at Break 145 %
145 %
IEC60811-1-1
Thermal Properties Metric English Comments
Oxygen Index 51 %
51 %