AlphaGary Megolon™ S552 Low Smoke Halogen Free

Category Polymer , Thermoplastic
Manufacturer AlphaGary
Trade Name Megolon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Megolon™ S552 Low Smoke Halogen Free.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Sheathing compound designed to meet VDE 0207 part 24 HM4. Good mechanical properties, fire performance and resistance to moisture. Designed to meet BS7655 LTS requirements. Application examples include Special Fire Survival / Power Medium Voltage.
Mechanical Properties Metric English Comments
Tensile Strength 14.0 MPa
2030 psi
Elongation at Break 200 %
200 %
IEC60811-1-1
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 138 °C
280 °F
Temperature Index
Oxygen Index 36 %
36 %