AlphaGary Vythene™ VYT/13E-55 CLEAR TL 0025 Polyurethane / Polyvinyl Chloride Compound

Category Polymer , Thermoplastic , Polyurethane, TP , Vinyl (PVC)
Manufacturer AlphaGary
Trade Name Vythene™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF AlphaGary Vythene™ VYT/13E-55 CLEAR TL 0025 Polyurethane / Polyvinyl Chloride Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Vythene™ is a polyurethane/PVC compound which combines the good properties of a thermoplastic elastomer with PVC. This unique compound provides flexibility, toughness, tear strength and abrasion resistance at an economical price. Good flexibility, toughness, tear strength and low temperature resistanceFormulated for extrusion
Mechanical Properties Metric English Comments
Hardness, Shore A 55
55
Typical
50 - 85
50 - 85
Optical Properties Metric English Comments
Transmission, Visible 90 %
90 %
Clear; thickness not specified
Descriptive Properties Value Comments
DEHP Free No
Phthalate Free No