Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Amco Plastic Materials
Trade Name PRIMATOP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Amco PRIMATOP PP CO 200 NB Impact Polypropylene Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PP CO 200 NB is cold temperature impact resistant, heat stabilized, and nucleated. Applications include toys and consumer products.Former A-Top Polymers product; part of Amco product line since 2013.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Index of Compound 20 g/10 min

@Load 2.16 kg,
Temperature 230 °C
20 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 80
80
ASTM D785
Tensile Strength, Yield 22.1 MPa
3200 psi
2 in/min; ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.5 in/min, Tangent Method; ASTM D790
Izod Impact, Notched 0.374 J/cm

@Temperature -30.0 °C
0.700 ft-lb/in

@Temperature -22.0 °F
ASTM D256
0.801 J/cm

@Temperature 0.000 °C
1.50 ft-lb/in

@Temperature 32.0 °F
ASTM D256
NB

@Temperature 22.8 °C
NB

@Temperature 73.0 °F
ASTM D256
Falling Dart Impact 28.2 J

@Temperature -30.0 °C
20.8 ft-lb

@Temperature -22.0 °F
0.5" Tup, 150"/sec; ASTM D3763
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 79.4 °C
175 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 43.3 °C
110 °F
ASTM D648