Aremco Pyro-Tape™ 682-ER High Temperature Tape Single layer polyimide film with silicone adhesive

Category Polymer , Adhesive , Tape
Manufacturer Aremco
Trade Name Pyro-Tape™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Aremco Pyro-Tape™ 682-ER High Temperature Tape Single layer polyimide film with silicone adhesive.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications Electrical Resistance Features Electrical insulation for process instrumentation, wiring and harnesses. RF induction coil insulation. Transformer, terminal and connector insulation. Masking gold fingers for printed circuit board wave soldering.
Physical Properties Metric English Comments
Thickness 63.5 microns
2.50 mil
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 260 °C
500 °F
Minimum Service Temperature, Air -73.3 °C
-100 °F
Electrical Properties Metric English Comments
Volume Resistivity 1.50e+17 ohm-cm
1.50e+17 ohm-cm
Dielectric Constant 3.4
3.4
Dielectric Strength 276 kV/mm
7000 kV/in
Descriptive Properties Value Comments
Adhesion 20 oz/in
Tape Tensile Strength 30 lbs/in