Arkema Group EVATANE® 33-15 Copolymer Ethylene - Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate
Manufacturer Arkema
Trade Name Evatane®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group EVATANE® 33-15 Copolymer Ethylene - Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVATANE® 33-15 is a random copolymer of Ethylene and Vinyl Acetate made by high-pressure radicalar polymerisation process. EVATANE® 33-15 is stabilized with antioxidants. The High Vinyl Acetate content of EVATANE® 33-15 brings softness, flexibility and polarity. EVATANE® 33-15 delivers high cohesive strength with any kind of fillers (HFFR compounds).Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.960 g/cc

@Temperature 23.0 °C
0.0347 lb/in³

@Temperature 73.4 °F
ISO 1183
Vinyl Acetate Content 30 - 33 %
30 - 33 %
FTIR (internal)
Melt Index of Compound 14 - 20 g/10 min

@Load 2.16 kg,
Temperature 190 °C
14 - 20 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 69
69
ASTM D2240
Tensile Strength at Break 15.0 MPa
2180 psi
ASTM D638
Elongation at Break 800 - 1000 %
800 - 1000 %
ASTM D638
Thermal Properties Metric English Comments
Melting Point 64.0 °C
147 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 0.999 kg
<= 104 °F

@Load 2.20 lb
ISO 306
Ring & Ball Softening Point 128 °C
262 °F
ASTM E28
Processing Properties Metric English Comments
Processing Temperature <= 230 °C
<= 446 °F