Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate

Category Polymer , Thermoplastic , Ethylene Vinyl Acetate , Ethylene Vinyl Acetate Copolymer (EVA), Film Grade
Manufacturer Arkema
Trade Name Evatane®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Evatane® 1003 VN 4 Ethylene Vinyl Acetate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
EVA copolymer made by high pressure tubular process. Applications Grade for transparent and thermal agricultural film for greenhouse coverage.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Density 0.935 g/cc
0.0338 lb/in³
Melt Flow 0.45 g/10 min

@Load 2.16 kg,
Temperature 190 °C
0.45 g/10 min

@Load 4.76 lb,
Temperature 374 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 6.00 MPa
870 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Tensile Modulus 0.0800 GPa
11.6 ksi
1 mm/min
Thermal Properties Metric English Comments
Melting Point 93.0 °C
199 °F
10°C/min
Vicat Softening Point 73.0 °C
163 °F
50°C/hr; 50N
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Users viewing this material also viewed the following: