Material Notes:
LOTRYL 37 EH 550 is a random copolymer of Ethylene and 2-Ethylhexyl Acrylate, prepared by the high pressure polymerization process. Co-monomer content is 37% in weight. LOTRYL 37 EH 550 is particularly recommended for the formulation of hot melt adhesives with low viscosity. LOTRYL 37 EH 550 is used as a viscosity modifier for technical polymers blends.Information provided by Arkema Group
Physical Properties Metric English Comments
Density 0.910 g/cc

@Temperature 23.0 °C
0.0329 lb/in³

@Temperature 73.4 °F
ISO 1183
Melt Index of Compound 550 g/10 min

@Load 2.16 kg,
Temperature 190 °C
550 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 62
62
ASTM D2240
Tensile Strength at Break 1.50 MPa
218 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 0.00600 GPa
0.870 ksi
ASTM D638
Thermal Properties Metric English Comments
Melting Point 72.0 °C
162 °F
DSC
Vicat Softening Point <= 40.0 °C

@Load 0.999 kg
<= 104 °F

@Load 2.20 lb
ASTM D1525
Descriptive Properties Value Comments
2-Ethylhexyl Acrylate Content (%) 37
IRTF (internal)