Arkema Group Lacovyl® PB 1302 H PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Arkema
Trade Name Lacovyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lacovyl® PB 1302 H PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACOVYL PB 1302 H is a vinyl chloride homopolymer manufactured by microsuspension polymerization process for the preparation of plastisols.It is specially designed for compact articles with low plasticizer content.* MAIN CHARACTERISTICS Viscosity index (IS0 1628-2):125 ml/g,(K value:70). * APPLICATIONSLACOVYL PB 1302 H is recommended for the following applications : high gloss and crystal clear surface coats, impregnation layer for floor coverings, compact coatings for wall covering and coated fabrics, foam layer for artificial leather, coating by mechanical foam techniques, rotomolding (toys, automotive industry, etc), dip molding, compact or foamed cap closures. ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 127 cm³/g
127 cm³/g
Viscosity Number