Arkema Group Lacovyl® PE 1312 PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Foam Grade
Manufacturer Arkema
Trade Name Lacovyl®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lacovyl® PE 1312 PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACOVYL PE 1312 is a vinyl chloride homopolymer manufactured by emulsion polymerization process for the preparation of high viscosity plastisols. It is particularly suitable for the manufacture of compact or foam coatings containing high plasticizer levels.* MAIN CHARACTERISTICS Viscosity index (ISO 1628-2):125 ml/g,(K value:70). * APPLICATIONSLACOVYL PE 1312 may be used in the following areas : flexible coated fabrics, leather cloths, extrudable mastics for cars, resilient low density foams, and as thickening agent to change the rheology of a product. ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 125 cm³/g
125 cm³/g
Viscosity Number