Material Notes:
LACOVYL S 071 S is a low molecular weight vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics :_ Viscosity index (ISO 1628-2):79 ml/g,(K value:57). Apparent density (ISO 60):0.58 g/ml. good low temperature fusion characteristics. suitable for dry blend preparation providing a controlled feed to production machines. excellent base color and thermal stability. Provides finished products with good transparency and free from fish eyes.* RECOMMENDED APPLICATIONS Bottles by extrusion and injection blow molding. LACOVYL is also recommended for biaxial orientation processes. Calendering of rigid sheet. Extrusion of rigid film and sheet. * EXAMPLES OF APPLICATIONSPVC-U: NAKAN RMA 705 N NAKAN RMS 501 L ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 79 cm³/g
79 cm³/g
Viscosity Number
Optical Properties Metric English Comments
Transmission, Visible 80 %
80 %
Mfr. reports 'Transparent' but doesn't quantify.
Users viewing this material also viewed the following: