Arkema Group Lacovyl® S 110 P PVC

Category Polymer , Thermoplastic , Vinyl (PVC) , PVC, Molded
Manufacturer Arkema
Trade Name Lacovyl®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Lacovyl® S 110 P PVC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LACOVYL S 110 P is a vinyl chloride homopolymer produced by a suspension polymerization process.Characteristics : Viscosity index (ISO 1628-2):112 ml/g,(K value:67). Apparent density (ISO 60):0.56 g/ml. molecular weight and morphology designed to give good processability with excellent mechanical properties. high tolerance of inorganic fillers in rigid PVC formulations. a very weak coloring of the resin after processing makes it possible to obtain profiles with regular color. * RECOMMENDED APPLICATIONS Extrusion of rigid profiles with improved mechanical properties (window frame, fencing etc...). Sheet extrusion. Extrusion of rigid pipe for all applications: water adduction, drainage, sewerage, conduit. ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Viscosity Test 112 cm³/g
112 cm³/g
Viscosity Number