Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Arkema Group Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Conditioned)

Category Polymer , Thermoplastic , Nylon , Nylon 12 , Nylon 12, Extrusion/Tubing Grade
Manufacturer Arkema
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arkema Group Rilsan® MA 4420 Nylon 12, Flexible Tubing Grade (Conditioned).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Designation ISO 1874-PA12-HI,EHL,22-003Flexible grade for tubes extrusion. Available color: black. Light and heat stabilized.Flexibility. High burst pressure and impact strength. Fit for use in a wide range of temperature. Very good chemical resistance.Example applications: Tubes for air brake system in trucks approved by ISO 7628, DIN 73378 (PA12-PHLY), NFR 12632, SAEJ 844.ISO data provided by the manufacturer, Arkema.
Physical Properties Metric English Comments
Melt Flow 4.8 g/10 min

@Load 2.16 kg,
Temperature 235 °C
4.8 g/10 min

@Load 4.76 lb,
Temperature 455 °F
Mechanical Properties Metric English Comments
Tensile Strength, Yield 31.0 MPa
4500 psi
50 mm/min
Elongation at Break >= 50 %
>= 50 %
Nominal Strain; 50 mm/min
Elongation at Yield 21 %
21 %
50 mm/min
Tensile Modulus 0.640 GPa
92.8 ksi
1 mm/min
Charpy Impact Unnotched NB
NB
NB
NB
Low Temp
Charpy Impact, Notched 2.79 J/cm²
13.3 ft-lb/in²
0.540 J/cm²

@Temperature -30.0 °C
2.57 ft-lb/in²

@Temperature -22.0 °F
Users viewing this material also viewed the following: