Arlon Ultrapad™ D 65 (55073R062) 0.0622 (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate

Category Polymer , Thermoset , Silicone , Silicone Rubber , Silicone, Molded, Glass Fiber Filled
Manufacturer Arlon
Trade Name Ultrapad™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Arlon Ultrapad™ D 65 (55073R062) 0.0622 (1.58 mm) Cured Silicone Rubber with Fiberglass Substrate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Description: Ultrapad™ D65 Silicone-based press pad. Arlon UltraPad press pad is a high performance, fiberglass reinforced, silicone sheet designed for flex and rigid-flex circuitry lamination. UltraPad press pad provides excellent pressure uniformity with good consistency and longevity throughout its service life. UltraPad press pads are the most cost effective press pad solution across a wide range of process pressures and temperatures.Design/Construction: Interleave: Polyethylene Side 1: Cured Silicone RubberSubstrate: Style 162 FiberglassSide 2: Cured Silicone Rubber Advantages:Consistent, reliable service life - predictable changeover schedule, higher yield (no lost loads)Uniform pressure over the entire laminate surface - higher yield, better quality laminateAvailable in softer low durometer variants - lower durometer > better pressure uniformityProduct Use: Press PadAppearance: Red silicone rubber on fiberglass clothThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arlon, Silicone Technologies Division
Physical Properties Metric English Comments
Density 1.09 g/cc
0.0394 lb/in³
Silicone Property; Arlon SQA-TMS-024
Thickness 74.9 microns
2.95 mil
Interleave
480 microns
18.9 mil
Substrate; Arlon SQA-TMS-003
551 microns
21.7 mil
Side 1; Arlon SQA-TMS-003
551 microns
21.7 mil
Side 2; Arlon SQA-TMS-003
1580 microns
62.2 mil
Overall; Arlon SQA-TMS-003
Mechanical Properties Metric English Comments
Hardness, Shore A 43
43
Silicone Property; ASTM D2240
65
65
Product Property; ASTM D2240
Tensile Strength 7.79 MPa
1130 psi
Silicone Property; ASTM D412
Elongation at Break 854 %
854 %
Silicone Property; ASTM D412
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 300 °C
572 °F
Processing Properties Metric English Comments
Shelf Life 60.0 Month

@Temperature 23.0 °C
60.0 Month

@Temperature 73.4 °F
From date of manufacture
Descriptive Properties Value Comments
Color Naturally White
Substrate
Red
Recommended Application Pressure 0 - 5 Mpa
Service Life (200°C and 2.07MPa)
(225°C and 2.07MPa)
(250°C and 2.07MPa)
Total Product Weight (g/m2) 1605
Arlon SQA-TMS-025