Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Asahi Glass ASAHIKLIN AK-225 Hydrochlorofluorocarbon Solvent

Category Fluid , Solvent
Manufacturer Asahi Glass Company
Trade Name ASAHIKLIN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass ASAHIKLIN AK-225 Hydrochlorofluorocarbon Solvent.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Asahilkin AK-225 is an environmentally sensible hydrochlorofluorocarbon (HCFC) designed to replace chlorofluorocarbon (CFC), perfluorocarbon (PFC), and other HCFCs with high ODP values in a variety of applications. Its selective solvency, physical properties, and ability to form azeotropes make AK-225 ideal for general and precision cleaning, as a carrier for silicone and halogenated lubricants, and as a coolant.It is thermally stable, nonflammable and recoverable by distillation with no decomposition. It has substantially lower global warming potential (GWP) than PFCs and HFCs and an extremely low ozone depletion potential (ODP). AK-225 is exempt from VOC regulations by the U.S. EPA as described in the Oct. 8, 1996 Federal Register.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Density 0.00778 g/cc

@Temperature 60.0 °C
0.000281 lb/in³

@Temperature 140 °F
Vapor (1 atm)
1.55 g/cc

@Temperature 25.0 °C
0.0560 lb/in³

@Temperature 77.0 °F
Liquid
Solubility of Water 0.031 %
0.031 %
25°C
Solubility in Water 0.033 %
0.033 %
25°C
Viscosity 0.59 cP

@Temperature 25.0 °C
0.59 cP

@Temperature 77.0 °F
Molecular Weight 202.94 g/mol
202.94 g/mol
Vapor Pressure 0.378 bar

@Temperature 25.0 °C
284 torr

@Temperature 77.0 °F
Surface Tension 16.2 dynes/cm
16.2 dynes/cm
25°C
Thermal Properties Metric English Comments
Heat of Vaporization 145 J/g
62.3 BTU/lb
b.p.
Specific Heat Capacity 0.724 J/g-°C

@Temperature 60.0 °C
0.173 BTU/lb-°F

@Temperature 140 °F
Vapor (1atm)
1.046 J/g-°C

@Temperature 25.0 °C
0.2500 BTU/lb-°F

@Temperature 77.0 °F
Liquid
Melting Point -131 °C
-204 °F
Boiling Point 54.0 °C
129 °F
Optical Properties Metric English Comments
Refractive Index 1.326

@Temperature 23.0 °C
1.326

@Temperature 73.4 °F
Electrical Properties Metric English Comments
Dielectric Constant 4.14

@Frequency 1e+6 Hz
4.14

@Frequency 1e+6 Hz
Chemical Properties Metric English Comments
Critical Pressure 29.62 bar
22220 torr
Critical Temperature 208 °C
406 °F
Critical Density 0.558 g/cc
0.0202 lb/in³
Descriptive Properties Value Comments
Global Warming Potential (CO2=1, 100yr ITH) 370
KB Value 31
Ozone Depletion Potential (CFC-11 = 1.0) 0.03
Ratio of Specific Heat Cp/Cv 60C 1atm 1.076
Relative Evaporation Rate (ether=100) 90
Solubility Parameter 7.3
Users viewing this material also viewed the following: