Asahi Glass Fluon® G192 PTFE Granular Powder

Category Polymer , Thermoplastic , Fluoropolymer , PTFE , PTFE Powder
Manufacturer Asahi Glass Company
Trade Name Fluon®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Fluon® G192 PTFE Granular Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Fluon®PTFE granular powders (molding powders) are used for the production of sheets, rods, billets and other general moldings.Information provided by Asahi Glass Company, Inc.
Physical Properties Metric English Comments
Bulk Density 0.460 g/cc
0.0166 lb/in³
Particle Size 25 µm
25 µm
Linear Mold Shrinkage 0.047 cm/cm
0.047 in/in
Diametrical Shrinkage
Mechanical Properties Metric English Comments
Tensile Strength at Break 41.0 MPa
5950 psi
JIS K6891
Elongation at Break 360 %
360 %
JIS K6891
Processing Properties Metric English Comments
Injection Pressure 16.0 MPa
2320 psi
Recommended Molding Pressure.
Descriptive Properties Value Comments
Compression Ratio 3.2