Asahi Glass Lumiflon FE-4300 Solvent Soluble Fluoropolymer

Category Polymer , Thermoplastic , Fluoropolymer
Manufacturer Asahi Glass Company
Trade Name Lumiflon
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Glass Lumiflon FE-4300 Solvent Soluble Fluoropolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Lumiflon was developed by Asahi Glass in 1982, and is unique being the first solvent soluble fluoropolymer. The FEVE based Lumiflon has a alternative copolymer. The complete inter-changeability between the Fluoroethylene and Alkyl Vinyl Ether gives excellent weathering and a high chemical resistance. FE-4300 is environmentally friendly and can be made into a durable coating for architectural applications.Information provided by Asahi Glass Company, Inc.