Asahi Kasei ASACLEAN PF Purging Compound

Category Polymer , Thermoplastic , Purging Compound
Manufacturer Asahi Kasei
Trade Name ASACLEAN
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Asahi Kasei ASACLEAN PF Purging Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Asaclean PF is formulated for super-engineering resins at processing temperatures of up to 420°C (790°F). PF Grade is suitable for Hot Runner cleaning. PF can be used as a sealing material during machine shutdowns within the temperature ranges of 280°-370°C (535°-700°F) due to its superior thermal stability.Information provided by Asaclean.